MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Flint Hills P5M4R-034 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.

Applications: Injection Molding: medical devices

Information Provided by Flint Hills Resources

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 12 g/10 min12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8383ASTM D785
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus, 1% Secant 740 MPa107000 psiASTM D790
Izod Impact, Notched 0.400 J/cm
@Temperature 23.0 °C
0.749 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact 26.0 J
@Temperature 23.0 °C
19.2 ft-lb
@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 790 MPa115000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pinnacle Polymers 3220 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 5135 C Clarified Polypropylene Random Copolymer, Injection Molding Grade
Pinnacle Polymers 1112 Polypropylene Homopolymer, Injection Molding Grade
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene
Chi Mei Polylac® PA-757 ABS

PFLINT027 / 104581

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.