MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 5863 Defoamer
Categories: Other Engineering Material

Material Notes: Product description: TEGOPREN 5863 is a polyether siloxane. It is a non-ionic product with 100 % active content.

Application: In paper application TEGOPREN® 5863 is recommended as defoamer booster for mineral or silicone oil based pulp defoamers and as emulsifier and booster for paper mill defoamers based on fatty alcohols. In textile application TEGOPREN® 5863 is re-commended as lubricant and wetting/spreading agent in non-polar systems. It is suitable for the treatment of fibers or fabrics applied by padding. TEGOPREN® 5863 provides good sew ability and lubricity. It can be used alone or in combination with other organo modified siloxanes or organic based surfactants.

Benefits: In paper application TEGOPREN® 5863 is re-commended as defoamer booster for mineral or silicone oil based pulp defoamers and as emulsifier and booster for paper mill defoamers based on fatty alcohols. In textile application TEGOPREN® 5863 is re-commended as lubricant and wetting/spreading agent in non-polar systems. It is suitable for the treatment of fibers or fabrics applied by padding. TEGOPREN® 5863 provides good sew ability and lubricity. It can be used alone or in combination with other organo modified siloxanes or organic based surfactants.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 - 1.05 g/cc
Viscosity 2000 - 3400 cP
Surface Tension 31 dynes/cm0.1% in water
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 65.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.445 - 1.455
 
Descriptive Properties
Appearanceliquid, colorless to pale straw/brownish
Cloud point41-45°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5885 Additive
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5852 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5851 Defoamer

PEVONIL598 / 196802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.