MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraton® D1153 A (SBS) Liner Block Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in the grade nomenclature:
Kraton D1153 AS - supplied as porous pellets dusted with amorphous silica
Kraton D1153 AT - supplied as porous pellets dusted with talc

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1153 A is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 2781
Bulk Density 0.400 g/ccASTM D 1895 method B
Volatiles <= 0.30 %KM 04
Viscosity 1400 - 1900 cP25% Toluene Solution at 25°C; KM 06
Molecular Weight 123000 g/molApparent, Triblock; BMS 0490
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Ash 0.10 - 0.40 %AS, AT; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 15.0 sec
Measured on compression molded slabs; ASTM D2240
Tensile Strength 28.0 MPameasured on films cast from a solution in toluene; ISO 37
Elongation at Break 800 %Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00290 GPa
@Strain 300 %
film cast from poluene solution; ISO 37
 
Descriptive Properties
ContentAntioxidant>0.1%, KM 08
 Polystyrene28.5-30.5%, KM 03
 Total Extractables<1.0%, KM 05
Triblock Content95 percentBMS 0490

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D2122 DO (SBS) Compound
Kraton® D1184 A (SBS) Branched Block Copolymer
Kraton® D1119 B (SIS) Linear Triblock Copolymer
Kraton® D1117 P (SIS) Linear Triblock Copolymer
Kraton® D1114 P (SIS) Linear Triblock Copolymer

PKRA9822 / 132721

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.