MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toray TORAYCON™ PBT Resin 1101G-30 Polybutylene Terephthalate (PBT), 30% Glass Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Reinforced, standard, GF30%. PBT-GF30.

General Toraycon™ Notes: TORAYCON™ PBT (polybutylene terephthalate) is a polyester-based thermoplastic engineering plastic with excellent electrical properties and chemical resistance. PBT resin is produced from the primary starting materials 1,4-butanediol and terephthalic acid and is a linear thermoplastic saturated polyester resin with ester bonds in the main chain. Unique features can be easily provided by compounding various additives, glass fibers, flame retardants, and utilizing solubilizing techniques. Furthermore, it is easy to add any color. The product is used in a large number of applications spanning several fields, including electrical and electronic devices, connectors and capacitor casing, automotive electronics, OA equipment, building materials, and industrial machinery parts.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccISO 1183
Water Absorption 0.070 %
@Time 86400 sec
In 23°C water; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm80x80x3mmt; Toray Method
Linear Mold Shrinkage, Transverse 0.010 cm/cm80x80x3mmt; Toray Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ISO 2039-2
Tensile Strength 145 MPaISO 527-1,2
Elongation at Break 2.5 %ISO 527-1,2
Tensile Modulus 10.2 GPaISO 527-1,2
Flexural Strength 220 MPaISO 178
Flexural Modulus 9.60 GPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²ISO 179
Charpy Impact, Notched 10.0 kJ/m²V-Notched; ISO 179
Coefficient of Friction 0.15Vs Metal; Suzuki Method
 0.19Vs Metal
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+16 ohm-cmIEC 60093
Dielectric Constant 3.7
@Frequency 5000 Hz
60% RH; IEC 60250
 4.2
@Frequency 1000 Hz
60% RH; IEC 60250
Dielectric Strength 914 V/milIEC 60243-1
Dissipation Factor 0.0020
@Frequency 5000 Hz
60% RH; IEC 60250
 0.020
@Frequency 1000 Hz
60% RH; IEC 60250
Arc Resistance 120 secW electrode; IEC 60950
Comparative Tracking Index 250 - 400 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 41.0 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 213 °CISO 75-1,2
Flammability, UL94 HB
@Thickness 0.800 mm
 
Descriptive Properties
Bar Flow (mm)96Toray Method. 250°C, 93 MPa, 1 mmt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY9063 / 248753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.