MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem Rubbermakers Sulfur MC Hot
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Rubbermakers Sulfur (MC Hot) is a treated grade of sulfur used to vulcanize rubber compounds. This non-dusting grade of treated Rubbermakers Sulfur provides the ultimate in dispersibility characteristics for a powder type sulfur. Its use is recommended for applications where excellent sulfur dispersion is essential.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.05 g/cc2.05 g/cc
Particle Mesh Size 200 Mesh200 Mesh99% thru
 325 Mesh325 Mesh90-95% thru
Ash 2.6 %2.6 %
 
Descriptive Properties
Content0.0001Acidity (as H2SO4)
Heat Loss0.0015
Purity0.964Sulfur Purity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH606 / 315524

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.