MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inov Chem Donpanel 423 CP/IP Base blend polyols for PIR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonPanel 423 system is a four components system which consists of blend polyols, polymeric MDI, catalyst and blowing agent (pentane series). The foam has good thermal insulation property, light in weight, high compression strength and flame retardant and other advantages. It is widely used to produce continuous sandwich panels, corrugated panels etc, which applies to make cold stores, cabinets, portable shelters and so on.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccK3-Cat 2816
 1.10 - 1.16 g/ccK1-blend polyols DonPanel 423
 1.24 g/ccK2-Polymeric MDI DD-44V80
Density 0.0330 - 0.0350 g/ccFree density, High pressure machine
 0.0340 - 0.0360 g/ccFree density, Manual Mix
 >= 0.0380 g/ccMold density; ISO 845
Water Absorption <= 3.0 %GB 8810
Viscosity 600 - 700 cPDynamic, K2-Polymeric MDI DD-44V80
 1200 - 1600 cPDynamic, K3-Cat 2816
 1800 - 2200 cPDynamic, K1-blend polyols DonPanel 423
Storage Temperature 10.0 - 25.0 °CK1-blend polyols DonPanel 423
 10.0 - 25.0 °CK2-Polymeric MDI DD-44V80
 10.0 - 25.0 °CK3-Cat 2816
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.120 MPaGB/T 8813
Adhesive Bond Strength >= 0.100 MPaGB/T 16777
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0240 W/m-K
@Temperature 15.0 °C
EN 12667
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CMaterial Temperature, Manual mix
 20.0 - 25.0 °CMaterial Temperature, High pressure machine
Mold Temperature 45.0 - 55.0 °CManual mixing
 45.0 - 55.0 °CHigh Pressure machine
Gel Time 0.670 - 1.00 minManual mixing
 0.670 - 1.00 minHigh pressure machine
Shelf Life 6.00 MonthK1-blend polyols DonPanel 423
 6.00 MonthK3-Cat 2816
 12.0 MonthK2-Polymeric MDI DD-44V80
 
Descriptive Properties
Appearancebrown transparent liquidK2-Polymeric MDI DD-44V80
 Light yellow to brown transparent liquidK1-blend polyols DonPanel 423
 Light yellow transparent liquidK3-Cat 2816
Closed-cell rate=90%ASTM D 2856
Cream time10-15 secManual mixing
 6-10 secHigh Pressure machine
Dimensional stability=0.5%24h, -30?; ISO 2796
 =1.0%24h, 100?; ISO 2796
FlammabilityLevel B2(Cannot Burn)DIN 4102
Hydroxyl value260-300 mgKOH/g
NCO content0.305K2-Polymeric MDI DD-44V80
Recommended Ratio100 gDonPanel 423
 1-3 gCat2816
 135-155 gPolymeric MDI DD-44V80
 7-10 gPentane (Cyclopentane/Isopentane)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM021 / 312550

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.