MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Kalix® 2855 High Performance (HPPA), 55% glass fiber
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: 55% glass fiber, high impact, higher strength, stiffness and ductility than 2955

Kalix® 2855 is a bio-sourced, polyamide-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and post-mold dimensional stability in thermoplastic parts. Its low viscosity and excellent flow properties make the material ideal for filling parts with thin-walled sections such as those encountered in the mobile electronics industry.

- Black: Kalix® 2855 BK 000
- White: Kalix® 2855 WH 000

Applications: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts

Features: Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Moisture Absorption; Low Warpage; Paintable; Platable

Typical values shown tested on Dry as Molded samples.

Standard Packaging and Labeling:
- Kalix® HPPA resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the product number, the color, the lot number, and the net weight.

Injection notes: Storage:
- Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Kalix® processing guide.
Drying:
- Kalix® HPPA is supplied in sealed bags. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts.
- Use of a desiccant dryer with -40°C dewpoint is strongly suggested to ensure Kalix® material has reached optimum moisture content before processing
Injection Molding:
- Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled.
- For light colors use lower melt temperature if possible. If operating in the 330°C melt temperature range, keep residence times below 5 minutes.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/cc
Water Absorption 0.090 %
@Time 86400 sec
0.090 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 cm/cm0.0015 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0058 cm/cm0.0058 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 230 MPa33400 psiISO 527-2
Elongation at Break 3.8 %3.8 %ISO 527-2
Tensile Modulus 19.0 GPa2760 ksiISO 527-2
Flexural Strength 355 MPa51500 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 95.0 kJ/m²45.2 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.77
@Frequency 2.40e+9 Hz
3.77
@Frequency 2.40e+9 Hz
Method B; ASTM D2250
Dissipation Factor 0.013
@Frequency 2.40e+9 Hz
0.013
@Frequency 2.40e+9 Hz
Method B; ASTM D2250
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 222 °C432 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FUnannealed; ISO 75-2/A
Glass Transition Temp, Tg 55.0 °C131 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 300 °C509 - 572 °F
Middle Barrel Temperature 280 - 330 °C536 - 626 °F
Front Barrel Temperature 280 - 330 °C536 - 626 °F
Melt Temperature 280 - 330 °C536 - 626 °FInjection
Mold Temperature 80.0 - 130 °C176 - 266 °F
Drying Temperature 80.0 °C
@Time 14400 - 43200 sec
176 °F
@Time 4.00 - 12.0 hour
Moisture Content <= 0.090 %<= 0.090 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorBlack; White
FormsPellets
ProcessingInjection Molding; Water-Heated Mold Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4301 / 280101

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.