MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DowAksa CarbonBond™ 300-UW Saturant Epoxy Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: DowAksa CarbonBond™ 300-UW Saturant Resin System is a fast-setting, general purpose epoxy laminating and bonding resin system that is well suited for use in performing repairs to various submerged structures or facilities in a freshwater or salt water environment. It has been found particularly useful in performing field repairs of pipes, poles, piles, tanks and other structures requiring a very fast set up and cure in the presence of water. The system may be used in high humidity situations and will cure in the presence of moisture.

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0381 lb/in³Part B
 1.15 g/cc0.0416 lb/in³Part A
Viscosity 1200 cP1200 cPPart A
 1500 cP1500 cPMixed
 2100 cP2100 cPPart B
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inASTM D2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ASTM D2240
Tensile Strength 66.2 MPa9600 psi14 Day Cure; ASTM D638
Elongation at Break 2.3 %2.3 %14 Day Cure; ASTM D638
Tensile Modulus 2.87 GPa416 ksi14 Day Cure; ASTM D638
Flexural Strength <= 102 MPa<= 14800 psi14 Day Cure; ASTM D790
Flexural Modulus 2.94 GPa427 ksiASTM D790
Compressive Strength 110 MPa15900 psiASTM D695
Izod Impact, Notched 0.737 J/cm1.38 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °FHDT load not reported, RT Cure
 93.3 °C200 °FHDT load not reported, Post-Cured
 
Processing PropertiesMetricEnglishComments
Gel Time 18.0 min18.0 min150g
 
Descriptive Properties
ColorAmberMixed
Mix Ratio100:22 A:BWeight
 4.2:1 A:BVolume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWAK992 / 287939

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.