MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DowAksa CFB20T Mid Weight Bidirectional Carbon Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: DowAksa CFB20T is a medium weight, high tensile strength bidirectional carbon fabric. It easily wets out with CarbonBond™ 300 Saturant Resin System and can be installed using the “wet lay-up” technique. This fabric has excellent mechanical properties.

CFB20T Carbon Fabric is designed to fabricate on-site composite reinforcements to a variety of structures and substrates: Flexural and shear reinforcement of beams; In-plane and out-of-plane reinforcement of concrete and masonry walls; Column wrapping and reinforcement of slab; Structural steel applications

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0650 lb/in³ISO 10119
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 710 ksiISO 10618
Elongation at Break 2.0 %ISO 10618
Tensile Modulus 34800 ksiISO 10618
 
Descriptive Properties
Weight20 oz/yd2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EDOWAK978 / 287925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.