MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 75 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Mylar® RL4 is designed to seal to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), polypropylene (PP), and polystyrene (HIPS).

The thickness of the heat seal layer and the heat seal strength of Mylar® RL4 is intermediate between Mylar® RL31 and Mylar® RL33. Mylar® RL4 and Mylar® RL32 produce similar heat seal strengths to most substrates, but Mylar® RL32 has a greater tendency to produce tearing seals while Mylar® RL4 tends to produce more peelable seals. Mylar® RL4 has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccCalculated from nominal thickness and yield
Moisture Vapor Transmission 0.750 cc-mm/m²-24hr-atmProc. E; ASTM E96
Oxygen Transmission 2.76 cc-mm/m²-24hr-atmTested per ASTM D3985 at 22°C
Thickness 0.750 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882
Film Elongation at Break, TD 80 %ASTM D882
Secant Modulus 3.79 GPaStiffness Modulus; ASTM D882
Tear Strength Test 1.9lb Graves; ASTM D1004
Film Tensile Strength at Break, MD 172 MPaASTM D882
Film Tensile Strength at Break, TD 241 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell UltRx 6000 CTFE Homopolymer, Barrier Film
DuPont Teijin Films Mylar® RL43T Polyester Packaging Film, 100 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
DuPont Teijin Films Mylar® 864 Polyester Packaging Film, 48 Gauge
DuPont Teijin Films Mylar® 850H Polyester Film, 80 Gauge

PDU7J0 / 33280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.