MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Southern Polymer PRIMALENE® WPP553E18 Vinyl Acetate Polyethylene
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: A high melt index vinyl acetate polyethylene

Typical Applications:

  • Extrusion coating
  • Heat seal layer
Features:
  • Outstanding heat sealability
  • High clarity
  • Good balance of drawability and neck-in

Information provided by Southern Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³
Vinyl Acetate Content 18.5 %18.5 %
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 190 °C
23 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 530 %530 %ASTM D882
Film Elongation at Break, TD 810 %810 %ASTM D882
Elmendorf Tear Strength MD 240 g240 gASTM D1922
Elmendorf Tear Strength TD 330 g330 gASTM D1922
Dart Drop Test 94.0 g0.207 lbASTM D1709A
Film Tensile Strength at Break, MD 21.6 MPa3140 psiASTM D882
Film Tensile Strength at Break, TD 15.0 MPa2170 psiASTM D882
1% Secant Modulus, MD 50.9 MPa7380 psiASTM D882
1% Secant Modulus, TD 55.3 MPa8020 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 83.9 °C183 °FPeak
Vicat Softening Point 53.9 °C129 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.90 %0.90 %ASTM D1003
Gloss 89 %89 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOUTH041 / 283897

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.