MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 150 Exxon Sawguide Oil
Categories: Fluid; Lubricant

Material Notes: EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system design and ambient temperatures. Your Exxon representative can assist in selecting the proper viscosity grade.

EXXON SAWGUIDE OIL is specially formulated to meet the lubrication requirements of modern gang saws and edgers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.889 g/cc
@Temperature 15.0 °C
Kinematic Viscosity at 40°C (104°F) 150 cSt
Kinematic Viscosity at 100°C (212°F) 16.4 cSt
ASTM Color 2.5ASTM D1500
 
Mechanical PropertiesOriginal ValueComments
Falex Load Test 0.0110 gLow Load, 600 lb for 2.5 hr
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 222 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.0037 %
 
Descriptive Properties
Rust Prevention, Distilled WaterpassASTM D665A
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON324 / 75749

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.