MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.

Mar-Bal standard grades can be injection, compression and transfer molded.

Information provided by Mar-Bal, Inc.

Vendors: Mar-Bal is the leading integrated compounder and molder of BMC Thermoset composite products and value added finishing services. Call 440-543-7526 or visit Mar-Bal.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 - 2.00 g/cc1.90 - 2.00 g/ccASTM D792
Bulk Factor 1.01.0ASTM D1895
Filler Content 10 %10 %Glass
Water Absorption 0.17 %
@Time 86400 sec
0.17 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.00050 - 0.0030 cm/cm0.00050 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 35 - 4835 - 48ASTM D2583
Tensile Strength 34.5 - 41.4 MPa5000 - 6000 psiASTM D638
Flexural Strength 96.5 - 110 MPa14000 - 16000 psiASTM D790
Flexural Modulus 13.8 - 15.2 GPa2000 - 2200 ksiASTM D790
Compressive Strength 103 - 124 MPa15000 - 18000 psiASTM D695
Shear Strength 41.4 - 48.3 MPa6000 - 7000 psiASTM D732
Izod Impact, Notched 1.33 - 1.87 J/cm2.50 - 3.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 12.6 kV/mm320 kV/inASTM D149
Arc Resistance >= 180 sec>= 180 secASTM D495
Track Resistance 3000 sec3000 secInclined-Plane Tracking; ASTM D2303
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
Flammability, UL94 HBHB
 
Descriptive Properties
Listed File E80533No

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound

PMARB902 / 149940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.