MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch Pad™ 819 Filament Tape Pads
Categories: Polymer; Adhesive

Material Notes: 3M™ ScotchPad™ Filament Tape Pad 819 is a pre-cut pad formed with layered high performance filament tape sheets featuring biaxially oriented polypropylene backing with continuous glass yarns that reinforce each sheet in both longitudinal and transverse directions. The adhesive on each sheet is specifically formulated to provide good adhesion to a wide variety of surfaces including metal, plastics, and fiberboard. Each piece of tape is coupled with a tab for easy handling and dispensing without the need for a dispenser. These sheets can be used for attaching, hinging, fastening, and sealing in many industrial, manufacturing and packaging applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 145 microns5.70 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 18.6 MPa2690 psiASTM D3759
Elongation at Break 6.0 %6.0 %ASTM D3759
Peel Strength 1.10 kN/m6.25 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypePressure sensitive synthetic rubber resin
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34134 / 168881

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.