MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Tecoflex® LM-95A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Tecoflex® LM-95A is an aliphatic polyether-based thermoplastic polyurethane (TPU).

Features: Low processing temperature with excellent physical properties

Process: Application requiring lower melt processing temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Tensile Strength at Break 50.0 MPaASTM D412
Elongation at Break 525 %
100% Modulus 1050 psi
@Strain 100 %
ASTM D412
300% Modulus 2350 psi
@Strain 300 %
ASTM D412
 
Processing PropertiesOriginal ValueComments
Zone 1 121 °CExtrusion
Zone 2 127 °CExtrusion
Zone 3 132 °CExtrusion
Zone 4 138 °CExtrusion
Adapter Temperature 138 °CExtrusion
Die Temperature 138 °CDie Zone 1
 138 °CDie Zone 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
Austin Novel Materials Innonen® H95A Polyester-based TPU Elastomer
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
Lubrizol LifeSciences Tecoflex® EG-72D-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Pellethane® 5863-85A TPU

PLUBR9076 / 203643

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.