MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sipol Technipol® 170 G Thermoplastic Adhesive Co-polyester
Categories: Polymer; Adhesive; Thermoplastic; Polyester, TP

Material Notes: Description: Technipol® 170/G is a co-polyester based thermoplastic adhesive designed for the production of oil and diesel filters in the automotive industry. Technipol® 170/G is characterized by a high chemical resistance (mineral oil and diesel vapors) and by a good thermal resistance.

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D 792
Viscosity 23 cP
@Temperature 230 °C
 24 cP
@Temperature 225 °C
 27 cP
@Temperature 220 °C
 30 cP
@Temperature 215 °C
 36 cP
@Temperature 210 °C
 49 cP
@Temperature 205 °C
Brookfield Viscosity 36 cP
@Temperature 210 °C
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Melt Flow 40 g/10 min
@Load 0.325 kg,
Temperature 210 °C
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 500 %ASTM D 638
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °CASTM D 3418
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CUnder Hopper
 170 - 190 °CCompression Zone
 180 - 210 °CMetering Zone
Feed Temperature 120 - 150 °C
Nozzle Temperature 200 - 220 °C
Die Temperature 200 - 220 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Suggested temperature profile for melters180-190°CPre-Heating Grills
 210-230°CTank
 220-230°CHose
 220-230°CNozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPOL006 / 297131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.