System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Akulon® K240-HP PA6-I, Dry, Heat Stabilized, Impact Modified, Extrusion Blow Molding
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Heat Stabilized
;
Nylon 6, Impact Grade
Material Notes:
Heat Stabilized, Impact Modified, Extrusion Blow Molding
Former DSM Engineering Plastics product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.10
g/cc
0.0397
lb/in³
ISO 1183
Water Absorption
9.0 %
9.0 %
Sim. ISO 62
Moisture Absorption
3.00 %
3.00 %
Humidity; Sim. ISO 62
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
70.0
MPa
10200
psi
ISO 527-1/-2
Elongation at Break
>= 50 %
>= 50 %
Nominal; ISO 527-1/-2
Elongation at Yield
4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus
2.50
GPa
363
ksi
ISO 527-1/-2
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
2.00
J/cm²
@Temperature -30.0 °C
9.52
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
5.00
J/cm²
@Temperature 23.0 °C
23.8
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
100
µm/m-°C
55.6
µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow
140
µm/m-°C
77.8
µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi)
170
°C
338
°F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
140
°F
ISO 75-1/-2
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Akulon® K240-HP PA6-I, Conditioned, Heat Stabilized, Impact Modified, Extrusion Blow Molding
Celanese Hostaform® T 1020 Extrusion Blow Molding Grade Acetal Copolymer
Envalior Akulon® Diablo HT-HG0 (K-X07029) (PA66+PA6)-GF50
Envalior Akulon® Diablo HT50-HPG5 (PA66+PA6)-GF25
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)
PDSM8065 / 184766
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.