MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Cookson Group STAYSTIK® 571 Silver Filled Electrically Conductive Film  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic

Material Notes: This thermoplastic adhesive film is designed for use in a variety of electronic applications. It is characterized by its excellent bonding at low process temperatures and extremely low ELASTIC MODULUS (60,000psi). The compliancy of this adhesive allows for the bonding of two materials having large dissimilarities in thermal expansion coefficients. The reworkability of this thermoplastic adhesive system offers many advantages in applications traditionally ill-suited to thermoset adhesives.

  • Fully polymerized resin - No "cure"
  • Easily reworkable - No outgassing
  • Bonds in seconds - Not hours or minutes
  • Low modulus reduces stress to bonded materials

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity >= 0.414 GPa>= 60.0 ksi
Adhesive Bond Strength >= 12.4 MPa>= 1800 psiDie shear adhesion, at 25°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00050 ohm-cm<= 0.00050 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity >= 3.00 W/m-K>= 20.8 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °FContinuous use
 <= 280 °C<= 536 °FExcursion Temperature
Minimum Service Temperature, Air -65.0 °C-85.0 °FContinuous use
Glass Transition Temp, Tg >= 25.0 °C>= 77.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Monthat 25°C
 
Descriptive Properties
Attach Temperature125-200°C
Filler MaterialSilver

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Furon® C695 Thermal Graphite Tape

PPLASK037 / 56327

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.