Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: Exact 3131 is an ethylene-based hexen plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3131 is designed for both monolayer and multilayer coextruded cast film applications requiring excellent toughness and heat sealing performance. Typical applications include heat seal layers in food packaging.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Cast Film
  • Industrial Packaging
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Thickness 25.4 microns1.00 mil
Melt Flow 3.5 g/10 min3.5 g/10 minExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 5.24 MPa760 psiASTM D882
Film Tensile Strength at Yield, TD 4.55 MPa660 psiASTM D882
Film Elongation at Break, MD 460 %460 %ASTM D882
Film Elongation at Break, TD 630 %630 %ASTM D882
Film Elongation at Yield, MD 10.3 %10.3 %ASTM D882
Film Elongation at Yield, TD 8.5 %8.5 %ASTM D882
Puncture Energy 61.8 J45.6 ft-lbExxonMobil Method
Elmendorf Tear Strength, MD 6.69 g/micron170 g/milASTM D1922
Elmendorf Tear Strength, TD 13.8 g/micron350 g/milASTM D1922
Dart Drop 41.3 g/micron1050 g/milASTM D1709A
Film Tensile Strength at Break, MD 73.70 MPa10690 psiASTM D882
Film Tensile Strength at Break, TD 60.8 MPa8820 psiASTM D882
1% Secant Modulus, MD 67.6 MPa9800 psiASTM D882
1% Secant Modulus, TD 74.5 MPa10800 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 93.9 °C201 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 76.0 °C169 °FExxonMobil Method
Vicat Softening Point 82.8 °C181 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.40 %0.40 %ASTM D1003
Gloss 93 %93 %ASTM D2457
 
Descriptive Properties
Puncture Force14 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 4150 Plastomer
ExxonMobil Escorene® LD 713.93 Cast Film Resin
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate
ExxonMobil LD 317.87 Film Resin
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin

PEXB347 / 37652

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.