MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® LX9110 black | PA12 Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Conductive polyamide 12 compound for use in multilayer tubing. VESTAMID LX9110 is a specially modified conductive polyamide 12 compound for manufacturing conductive multilayer tubing. It is used in multilayer tubing MLT 4540.1 developed by Evonik Degussa GmbH. Compared to common conductive compounds VESTAMID LX9110 is charac­terized by a lower melt viscosity and thus excellent extrudability also in thin layers. Using VESTAMID LX9110 tubing features an excellent inner surface quality. Multilayer tubing with an innermost layer made of VESTAMID LX9110 complies with the American automotive manufacturers’ requirements to avoid electrostatic charging generated by fuel flow. VESTAMID LX9110 is supplied as ready-to-process pellets in moisture-proof bags.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Water Absorption 1.5 %Sim. to ISO 62
Moisture Absorption 0.500 %Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.0 MPaISO 527
Elongation at Break 115 %Nominal; ISO 527
 132 %ISO 527
Tensile Modulus 640 MPaISO 527
50% Modulus 0.0320 GPa
@Strain 50 %
ISO 527
Flexural Strength 13.0 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 560 MPaISO 178
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 90.0 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 47 ohm-cmIEC 62631-3-1
 47 ohm-cmOn bar, ?V; IEC 62631-3-1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1/-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® LX9112 Nylon 12
Evonik VESTAMID® EX9203 black Nylon 12
Evonik VESTAMID® LX9102 PA 12
Evonik Vestamid® L1723 Plasticized Nylon 12
Evonik Vestamid® L1670 Nylon 12

PEVONIK864 / 243071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.