MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller 1527B RTV silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: 1527B is a black, medium viscosity, low odor and good workability RTV silicone. Cures at room temperature when exposed to moisture. Excellent flexibility, adhesive property, electrical insulation, weather resistance, aging resistance and thermal cycle resistance. 1527B passes FDA 21 CFR 177.2600 and is UL94 certified.

Features and Benefits:

  • Excellent heat resistance properties
  • Wide operating temperature range
  • Easy to use for reworkable applications
  • Fast setting one component material
  • Neutral cure low/no odor
  • UL94 rated
  • Meets FDA 21 CFR 177.2600
Typical Applications:
  • Appliances
  • Ovens
  • Cook Tops
  • Microwave Ovens
  • Glass Bonding
  • Solar Cells
  • Lighting Systems
  • Battery Sealing

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 40000 - 70000 cP
Storage Temperature 8.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28GB/T 531
Tensile Strength 1.50 MPaGB/T 528
 1.50 MPa
@Temperature <=175 °C,
Time 605000 sec
Damp Heat Aging Testing; 85% RH; GB/T 528
Elongation at Break 180 %GB/T 528
 180 %
@Temperature <=175 °C,
Time 605000 sec
Damp Heat Aging Testing; 85% RH; GB/T 528
Shear Strength 1.50 MPaLap Joint, Aluminum; GB/T 7124
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 ohm-cmGB/T1692
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 30.0 minTack Free Time
 24.0 hour
@Thickness >=2.00 mm
Full Cure
 
Descriptive Properties
ColorBlack
ConsistencyThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL103 / 316894

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.