MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

PolyPLASTY PolyJARID Antistatic Alkaline Polyamide 6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Polyamides are semi-crystalline thermoplastics, the properties of which depend very strongly on the water content . Their balanced characteristics make Polyamides one of the most widely used plastics in engineering.

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³
Moisture Absorption at Equilibrium 2.5 %2.5 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 77 - 8777 - 87
Tensile Strength >= 45.0 MPa>= 6530 psi
Elongation at Break 10 - 30 %10 - 30 %
Modulus of Elasticity 3.20 GPa464 ksi
Charpy Impact Unnotched 57.0 J/cm²271 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²
Coefficient of Friction 0.30 - 0.350.30 - 0.35
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 8.00 - 10.0 µm/m-°C4.44 - 5.56 µin/in-°F
Thermal Conductivity 0.300 - 0.350 W/m-K2.08 - 2.43 BTU-in/hr-ft²-°F
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYPL919 / 197629

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.