Silver/Carbon Paste is used for printing tracks where a higher resistance is needed instead is of using a pure silver paste. This paste has a reduced level of silver and higher level of Carbon in comparison with C2060428D3. Therefore this paste has a much higher resistance then C2060428D3. Product Benefits: It contains a crosslinking resin system for printing on substrates with low adhesion surfaces, ie Polyimide |