System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical LUPOL GP3400 PP+MF40%
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Mineral Reinforced
Material Notes:
Description: Injection Molding, PP+MF30%, General Purpose
Application: Electrical, Electronic and Automotive Interior Parts
CAS: 9003-07-0 and 14807-96-6
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.20
g/cc
ASTM D792
Maximum Moisture Content
0.010
Injection Molding
Linear Mold Shrinkage, Flow
0.0060
-
0.011
cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow
10
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
340
kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break
10 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength
570
kg(f)/cm²
@Thickness 6.40 mm
1.3mm/min; ASTM D790
Flexural Modulus
44000
kg(f)/cm²
@Thickness 6.40 mm
1.3mm/min; ASTM D790
Izod Impact, Notched
>=
2.50
kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
140
°C
@Thickness 3.20 mm
Unannealed; ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
190
-
210
°C
Injection Molding
Middle Barrel Temperature
200
-
230
°C
Injection Molding
Front Barrel Temperature
200
-
230
°C
Injection Molding
Nozzle Temperature
210
-
230
°C
Injection Molding
Melt Temperature
200
-
230
°C
Injection Molding
Mold Temperature
40.0
-
60.0
°C
Injection Molding
Drying Temperature
70.0
-
80.0
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
Back Pressure
29.4
-
58.8
MPa
Injection Molding
Screw Speed
30
-
60
rpm
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Addiplast Addilene H 220 M40 Polypropylene Homopolymer
ExxonMobil PP1043F Mineral-filled Homopolymer
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced
Avient Maxxam™ NT-818.B001-8000 Polypropylene
Avient Maxxam™ DP-9156-5-8000 Polypropylene Copolymer (PP Copolymer)
PLAY474 / 148484
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.