SABIC® PPcompound S3625 is a 25% short glass fiber reinforced polypropylene copolymer compound for injection moulding applications. The compound is UV stabilized and the glass fibers are chemically coupled to the PP matrix. This compound combines a matt surface, good sound dampening and excellent scratch resistance with soft-touch haptics and is especially designed for aesthetical automotive interior applications.
SABIC® PPcompound S3625 is a designated automotive grade.
IMDS ID: 559182813Information provided by SABIC |