- Available in North America
- Filler: Glass Fiber Reinforcement, 13% Filler by Weight
- Additive: Heat Stabilizer and Lubricant
- Features: Lubricated and Heat Stabilized
- RoHS Compliant
- Form: Pellets
- Processing Method: Injection Molding
- Color: Black
Information provided by Ravago. |