MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lotte Advanced Materials TITANEX HB0976 HDPE, Blow Molding, Film Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded; High Density Polyethylene (HDPE), Film Grade

Material Notes: HB0976 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for blow molding. HB0976 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.

Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and cosmetic containers.

Advantages: Excellent stress crack resistance, excellent resistance to most chemicals and outstanding rigidity with balanced impact strength and stiffness, high melt strength and moderate die swell.

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D1505
ESCR 10% Igepal® >= 250 hour>= 250 hourF50; ASTM D1693
Melt Flow 0.100 g/10 min0.100 g/10 minI2; ASTM D1238
 8.00 g/10 min8.00 g/10 minI21; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 390 MPa56600 psiASTM D638
Tensile Strength, Yield 32.4 MPa4690 psiASTM D638
Elongation, Ultimate >= 700 %>= 700 %ASTM D638
Flexural Modulus 1.18 GPa171 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 °C356 °FRear zone temperature setting
 190 °C374 °FFront zone temperature setting
Die Temperature 190 °C374 °F
Head Temperature 190 °C374 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9598 / 326080

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.