MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Reynolds duoMatrix™ NEO Polymer modified gypsum system
Categories: Other Engineering Material

Material Notes: Product Overview: duoMatrix™ NEO is a versatile polymer modified gypsum system that has superior physical and performance properties compared to regular gypsum products. Part A is powder and Part B is liquid. The mix ratio of NEO is a convenient 2A:1B by volume. NEO is easy to use and can be cast solid, slush cast, rotationally cast, laid up by hand with chopped glass fiber or sprayed. NEO can be thickened using Matrix™ Thickener, accelerated using Matrix™ Accelerator and slowed using Matrix™ Retarder. Fully cured pieces are strong, water-resistant and can be painted, sanded, machined and more. NEO certifies to the highest flame rating (UL-94V-O / ASTM E-84 - Class A), making it suitable for public space applications including creating themed environment elements, architectural elements, sculpture and more. Versatility – NEO can take you in many creative directions by allowing you to make a variety of finish effects including different colors, metallics, glitters, stone and more (see Creating Finished Effects section).

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.584 g/cc
Water Absorption <= 0.50 %after 24 hour water soak
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3300 - 5500 psi
Flexural Strength 7500 - 9800 psi
Compressive Strength 6500 - 9500 psi
Tensile Impact Strength 175 ft-lb/in²
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 90.0 minDrill Mixed
Pot Life 30.0 minDrill Mixed
 
Descriptive Properties
ColorWhite
Freeze/Thaw Resistance300 cycles
Mix Ratio100:50Powder: Liquid by weight or volume
Specific Volume17.45[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN318 / 297019

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.