MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Keltan® 2750 Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Amorphous ethylene-propylene rubber with high ENB (ethylidene norborene) content and low Mooney viscosity. The high ENB content enables fast and efficient network formation resulting in excellent physical properties. Typical application areas are high hardness automotive profiles and corner molds.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³
Mooney Viscosity 28
@Temperature 125 °C
28
@Temperature 257 °F
(1+4); ISO 289
 
Descriptive Properties
Content48 percentEthylene, ASTM D3900
 7.8 percentENB, ASTM D6047

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Keltan® 3050 Ethylene-Propylene Rubber
Lanxess Keltan® 2470L Ethylene-Propylene Rubber
Lanxess Keltan® 3973 Ethylene-Propylene Rubber
Lanxess Keltan® 6675 EPDM Rubber
Lanxess Keltan® 2450S Ethylene-Propylene Rubber

PLANY8558 / 208951

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.