MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Petropol Thanelene® A3 80A HL NTLA010 TP324 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: Hardness 80 shore A, Plasticized, Thermoplastic Polyurethane

Resin ID (ISO 1043): TPU
Additive: Plasticized
Processing: Injection Molding, Extrusion
Color: Natural

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 - 1.26 g/cc0.0441 - 0.0455 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 77 - 8377 - 83DIN 53505
Tensile Strength at Break >= 35.0 MPa>= 5080 psiDIN 53504
Elongation at Break >= 650 %>= 650 %DIN 53504
Flexural Strength  >= 4.00 MPa
@Strain 100 %
>= 580 psi
@Strain 100 %
DIN 53504
 >= 8.00 MPa
@Strain 300 %
>= 1160 psi
@Strain 300 %
DIN 53504
Tear Strength >= 65.0 kN/m>= 371 pliDIN 53515
Abrasion <= 40<= 40[mm3]; DIN 53505
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 190 °C338 - 374 °FMolding
Drying Temperature 100 °C212 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL400 / 313308

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.