MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Methyl isocyanate, CH3CNO
Categories: Fluid; Solvent

Key Words: CH3CNO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/cc
@Temperature 20.0 °C
Viscosity 1.0 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 57.052 g/mol
Vapor Pressure 348.289 torr
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 55.0 atm
Critical Temperature 218 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 518.5 J/g
Thermal Conductivity 0.1322 W/m-K
@Temperature 20.0 °C
Melting Point -45.0 °C
Boiling Point 38.9 °C
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.3258
Antoine's Vapor Pressure B Parameter2480.37
Antoine's Vapor Pressure C Parameter-56.31
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)624-83-9
Chemical FormulaCH3CNO
Critical Compressibility (Zc)0
Molar Heat Capacity (298K)J/mol-K
Molar Heat Capacity of Vapor a Parameter33.472
Molar Heat Capacity of Vapor b Parameter2267.728
Molar Heat Capacity of Vapor c Parameter0.1039
Molar Heat Capacity of Vapor d Parameter-5.816E-06
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

VORGS229 / 99593

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.