MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Anderman Ceramics EA96 Sintered Alumina, 96%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: High strength alumina (96%) available pink or white. Available in many shapes and sizes.

Information provided by Anderman Ceramics.

Key Words: Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.65 g/cc0.132 lb/in³
Open Porosity 0.00 %0.00 %Gas Tight
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 9.09.0
Tensile Strength 131 MPa19000 psi
Flexural Strength 310 MPa45000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.00e+6 ohm-cm
@Temperature 600 °C
1.00e+6 ohm-cm
@Temperature 1110 °F
 1.00e+14 ohm-cm
@Temperature 20.0 °C
1.00e+14 ohm-cm
@Temperature 68.0 °F
Dielectric Constant 9.3
@Frequency 1e+6 Hz
9.3
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.50 µm/m-°C
@Temperature 20.0 - 1000 °C
4.17 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 23.0 W/m-K
@Temperature 20.0 - 100 °C
160 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 1600 °C2910 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 96 %96 %
B2O3 <= 0.010 %<= 0.010 %
CaO 0.020 %0.020 %
Fe2O3 0.010 %0.010 %
MgO 0.020 %0.020 %
Na2O 0.14 %0.14 %
SiO2 3.6 %3.6 %
 
Descriptive Properties
Thermal Shock ResistanceMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EA998 Sintered Alumina, 99.8%
Anderman Ceramics EA95 Sintered Alumina, 95%
Anderman Ceramics EA999 Sintered Alumina, 99.9%
MarkeTech Aluminum Oxide Ceramic - Alumina 96%
Alumina, alpha Al2O3, 96%

CANDER02 / 475

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.