MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® TPE A 5904 LC BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and feature excellent heat and ozone resistance. LC products cover a wide temperature span from -40°F to 300°F. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5910 sec; ASTM D-2240
Tensile Strength, Ultimate 5.80 MPaASTM D638
Elongation at Break 950 %ASTM D638
100% Modulus 0.00230 GPa
@Strain 100 %
ASTM D638
300% Modulus 0.00469 GPa
@Strain 300 %
ASTM D638
Tear Strength 26.3 kN/mASTM D624
Compression Set 29 %
@Temperature 70.0 °C
for 70 hours at 70°C; ASTM 395
 45 %
@Temperature 100 °C
70 hours at 100°C; ASTM 395
 17 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM 395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Teknor Apex Telcar® OBC 2419A Thermoplastic Elastomer
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
ATI Allegheny Ludlum H13 Tool Steel, UNS T20813
Multibase Multi-Flex® TPE A 8002 BLK

PLA023 / 49484

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.