MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Mineral Filled

Material Notes: Starflam PK0069 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding Resin (also known as Starflam PA6 30E6 Z88)

Former Eurostar product. Eurostar has been acquired by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.66 g/ccDAM; ISO 1183
Water Absorption 0.80 %
@Time 86400 sec
DAM; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 63.0 MPaDAM; ISO 527-2
Elongation at Break 1.5 %DAM; ISO 527-2
Tensile Modulus 6200 MPaDAM; ISO 527-2
Flexural Strength 101 MPaDAM; ISO 178
Flexural Modulus 7400 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 193 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 130 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 65.0 °C
@Thickness 1.50 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 1.50 mm
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 1.50 mm
UL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 250 °CInjection
Middle Barrel Temperature 250 - 260 °CInjection
Front Barrel Temperature 250 - 270 °CInjection
Melt Temperature 250 - 270 °CInjection
Mold Temperature 50.0 - 90.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesFlame Retardant
 Halogenated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY
Envalior Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
Envalior Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond)
Envalior Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond)
Celanese Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)

PEUROSTA08 / 172022

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.