TABOREN-PC 62 T 50 is a compound based on polypropylene copolymer , filled with 50% of talc filler and stabilized with a basic additive package. It is designed for injection molding technology and used in applications requiring outstanding performance under enhanced temperatures.Information provided by Silon US LLC. |