MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® F136 PA6, Very High Viscosity, Film Extrusion
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Very High Viscosity, Film Extrusion

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Vapor Transmission 35.0 g/m²/dayDIS 15106-1/-3
Oxygen Transmission 1.35 cc-mm/m²-24hr-atm0% RH; DIS 15105-1/-2
 1.95 cc-mm/m²-24hr-atm85% RH; DIS 15105-1/-2
Viscosity 2250 cP
@Temperature 260 °C
Melt; DSM Method
 50 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
 50 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
 50 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
 900 cP
@Shear Rate 100 1/s,
Temperature 280 °C
 1000 cP
@Shear Rate 100 1/s,
Temperature 260 °C
 1030 cP
@Shear Rate 100 1/s,
Temperature 240 °C
 1030 cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
 1200 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
 1300 cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
Viscosity Number 245 cm³/gISO 307, 1157, 1628
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 34.0 MPaISO 527-3
Film Elongation at Break, MD 350 %ISO 527-3
Modulus of Elasticity 0.450 GPa50 mm/min; DSM Method
Coefficient of Friction, Dynamic 1.0ISO 8295
Tear Strength Test 32Trouser Tear resistance, parallel; ISO 6383-1
Film Tensile Strength at Break, MD 83.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 1.55 J/g-°C
 2.25 J/g-°C
@Temperature 20.0 - 150 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 83 %DSM Method
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 °CExtruder
Die Temperature 270 °C
Roll Temperature 110 °CChill
 
Descriptive Properties
Puncture resistance1400 J/mDSM Method
RSV formic acid3.6[1g/100ml], DSM Method
Type of extrusionCast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® REX 734™ UNS S31675 Specialty Steel
Akro-Plastic Akromid® B3 1 black (2501) PA 6 Dry, Heat Stabilized
BASF Ultramid® B27 03 PA6
BASF Ultramid® B40 L PA6
BASF Ultramid® B40 LN PA6

PDSM8011 / 184712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.