MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
California Fine Wire Nickel 271 Super Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Pure Element

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50000 psiAnnealed
 100000 psiStress relieved
 125000 psiHard
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 45.0 ohm-cir-mil/ft3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 59.0 W/m-K
Melting Point 2610 °F
Maximum Service Temperature, Air 500 °COperating Temperature
 
Component Elements PropertiesOriginal ValueComments
Nickel, Ni 99.97 %
 
Descriptive Properties
MagneticStrong
Temperature Coefficient of Resistance0.0065 ohms/ohm-°C0-100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
California Fine Wire Nickel 272 Super Alloy
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600
ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy
ATI Allvac® Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
California Fine Wire Nickel Alloy 99

NCALZ05 / 15548

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.