MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tempia Polylactic acid (PLA) Resin
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: A bio-degradable plastic, Polylactic acid (PLA) is made from corn. Products produced are compostable within 45 – 120 days. The degradation process of the item is temperature, humidity and thickness dependent. PLA’s good rigidity allows them to be a possible replacement for Polystyrene, ABS & PET. High heat reistance. Low taste transfer. High Gloss. Oil resistant.

Common Applications include: Cups, Disposable Goods, Packaging, Packaging, Food, Autmotive Interiors, Medical, Bags, Bottles. Food Service Applications.

Information provided by Plastic Service Center.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/cc
Water Absorption 0.13 %
Linear Mold Shrinkage 0.0040 cm/cm
Melt Flow 5.8 - 20 g/10 min
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 310 °F
Middle Barrel Temperature 340 - 380 °F
Front Barrel Temperature 355 - 400 °F
Nozzle Temperature 340 - 402 °F
Melt Temperature 390 - 393 °F
Mold Temperature 75.0 - 77.3 °F
Drying Temperature 212 °F
Dry Time 4 hour
Moisture Content 0.010 - 0.025 %
 
Descriptive Properties
CAS Number9051-889-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA
SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin
Lotte Advanced Materials Infino® AE-2030 PC/PET, General Purpose
SABIC HC 050 Amorphous Polyethylene Terephthalate

PTEMPIA00 / 70059

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.