MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Guang Dong LH-PP668 Antistatic PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Application Field: Suitable for injecting turnover box, hollow sheet, extruding sheet, tubes and pipes, blistering box

Feature: Good toughness, low water absorption, surface glossiness, good bending fatigue resistance, and easy to process molding

Grade: Injection

Color: Natural color, color matching is available

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.20 g/cc1.00 - 1.20 g/ccASTM D792
Melt Flow 0.20 - 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.20 - 1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238-L
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 MPa2900 psiASTM D638
Flexural Strength 40.0 - 45.0 MPa5800 - 6530 psiASTM D790
Flexural Modulus 1.965 - 2.003 GPa285.0 - 290.5 ksiASTM D790
Tensile Impact Strength 96.0 - 102 kJ/m²45.7 - 48.5 ft-lb/in²ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+8 - 1.00e+9 ohm1.00e+8 - 1.00e+9 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 85.0 °C185 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON007 / 283955

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.