MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Sanicro 60 Welding wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sanicro 60 welding wire is suitable for joining nickel-chromium-molybdenum Nickel alloys and chromium-nickel-molybdenum steels with very high corrosion resistance, such as Sandvik 254 SMO , Sanicro 63 and corresponding grades. It is also suitable for joining stainless steels and nickel alloys for high-temperature service. Sanicro 60 can also be used for dissimilar joining of stainless steels to nickel alloys and for overlay welding. Sanicro 60 is available as wire and rods.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 220220
Tensile Strength, Ultimate 770 MPa112000 psi
Tensile Strength, Yield 430 MPa
@Strain 0.2 %
62400 psi
@Strain 0.2 %
Elongation at Break 42 %42 %
Reduction of Area 51 %51 %
Charpy Impact  70.0 J
@Temperature -196 °C
51.6 ft-lb
@Temperature -321 °F
 150 J
@Temperature 20.0 °C
111 ft-lb
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 400 °C
6.67 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity  15.0 W/m-K
@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 16.0 W/m-K
@Temperature 100 °C
111 BTU-in/hr-ft²-°F
@Temperature 212 °F
 18.0 W/m-K
@Temperature 300 °C
125 BTU-in/hr-ft²-°F
@Temperature 572 °F
 22.0 W/m-K
@Temperature 500 °C
153 BTU-in/hr-ft²-°F
@Temperature 932 °F
 25.0 W/m-K
@Temperature 700 °C
174 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %Filler metal
 <= 0.030 %<= 0.030 %All-weld metal
Chromium, Cr 22 %22 %Filler metal
 22 %22 %All-weld metal
Iron, Fe 0.50 %0.50 %All-weld metal
 <= 1.0 %<= 1.0 %Filler metal
Manganese, Mn 0.20 %0.20 %Filler metal
 0.20 %0.20 %All-weld metal
Molybdenum, Mo 9.0 %9.0 %Filler metal
 9.0 %9.0 %All-weld metal
Nickel, Ni >= 60 %>= 60 %Filler metal
 60 %60 %All-weld metal
Niobium, Nb (Columbium, Cb) 3.4 %3.4 %All-weld metal
 3.5 %3.5 %Filler metal
Phosphorus, P <= 0.015 %<= 0.015 %Filler metal
 <= 0.015 %<= 0.015 %All-weld metal
Silicon, Si 0.20 %0.20 %Filler metal
 0.20 %0.20 %All-weld metal
Sulfur, S <= 0.010 %<= 0.010 %Filler metal
 <= 0.010 %<= 0.010 %All-weld metal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5258 / 199822

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.