MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

The Chemical Company FCC Food Grade DL-Malic Acid, C4H4O4
Categories: Fluid

Material Notes: Malic Acid is an organic compound with little to no odor, a dicarboxylic acid that is the active ingredient in many sour and tart foods. Malic Acid is generated during fruit metabolism and occurs naturally in all fruits and many vegetables. The pleasant, refreshing experience of biting into a juicy apple or cherry is partly caused by Malic Acid. Its mellow, smooth, persistent sourness can be blended with multiple food acids, sugars, high intensity sweeteners, flavors and seasonings to create distinctive taste experiences in foods, beverages and confections. Malic Acid is formed in metabolic cycles in the cells of plants and animals, including humans. The compound provides cells with energy and carbon skeletons for the formation of amino acids. The human body produces and breaks down relatively large amounts of Malic Acid every day. Malic Acid contributes to the sourness of green apples. It is present in grapes and gives a tart taste to wine. When added to food products, Malic Acid is the source of extreme tartness. It is used with or in place of the less sour citric acid in sour sweets. Malic Acid is used as a flavor enhancer in food preparation for confectionaries, beverages, fruit preparations and preserves, desserts, and bakery products. It is also essential in the preparation of medical products such as throat lozenges, cough syrups, effervescent powdered preparations, toothpaste and mouthwash. Additionally, Malic Acid is used in the manufacture of skin care products to rejuvenate and improve skin conditions.
Molecular Formula: C4H4O4

Information provided by The Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solubility in Water >= 99.9 %>= 99.9 %
Loss On Ignition >= 99.95 %>= 99.95 %
Particle Mesh Size 10 Mesh10 MeshGranular-100%
 25 Mesh25 MeshFine Granular< 99%
 50 Mesh50 MeshGranular< 10%, Powder> 75%
 100 Mesh100 MeshFine Granular< 5%
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.30 %<= 0.30 %Weight percent
 
Component Elements PropertiesMetricEnglishComments
Arsenic, As <= 0.00010 %<= 0.00010 %
Lead, Pb <= 0.00020 %<= 0.00020 %Heavy Metals (as Pb), 10ppm max
 
Descriptive Properties
AppearanceWhite crystalline granular/fine granular/powder
Assay= 99.5%on dry basis, as DL Malic Acid
Fumaric Acid (wt%)< 1.0
Hazen Color Value (pt-co)< 1010% solution
Maleic Acid (wt %)< 0.05
Specific Rotation-0.10° to 0.10°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTCC009 / 106998

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.