MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Terves TervAlloy™ 1331 Low Salinity Dissolvable Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: TervAlloy™ 1331 is the latest freshwater low temperature version of Terves’ patented dissolvable magnesium for oil and gas applications. This new alloy successfully bridges the gap between existing low salinity alloys and true freshwater-dissolvable alloys. TervAlloy 1331 is unique in that it has the dissolution characteristics of our TervAlloy 1530 (FW), but unlike 1530, is available in both tubulars and solids, and offers mechanical performance not only superior to our 1530 product. TervAlloy 1331 can be purchased in the same variety of shapes offered across the TervAlloy range (including cost-saving tubulars) in lengths up to 48 inches (in increments of 6 inches), and also in frac ball configurations up to 4.95 inches in diameter.

Information provided by Terves Incorporated

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 221 MPa32000 psi4" Solid Rod, 5:1 Extrusion Ratio
Tensile Strength, Yield 152 MPa22000 psi4" Solid Rod, 5:1 Extrusion Ratio
Elongation at Break 5.0 %5.0 %4" Solid Rod, 5:1 Extrusion Ratio, Longitudinal values
Compressive Strength 415 MPa60200 psi4" Solid Rod, 5:1 Extrusion Ratio
Shear Strength 129 MPa18700 psi4" Solid Rod, 5:1 Extrusion Ratio
 
Descriptive Properties
Dissolution Data20 mg/cm2hr0.1% KCl, 60°C
 30 mg/cm2hr1.0% KCl, 60°C
 33 mg/cm2hr3% KCl, 60°C
 5 mg/cm2hr0.1% KCl, 30°C
 50 mg/cm2hr0.1% KCl, 90°C
 69 mg/cm2hr1.0% KCl, 90°C
 76 mg/cm2hr3% KCl, 90°C
 8 mg/cm2hr3% KCl, 30°C
 8 mg/cm2hr1.0% KCl, 30°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTERVES011 / 314478

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.