MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Petropol Nypol® B3 TZ PRTA011 NT381 Nylon 6, Impact Modifier
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Product Description: Impact Modified, Polyamide 6

Resin ID (ISO 1043): PA6
Additive: Impact Modifier
Processing: Injection Molding
Color: Black

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psiISO 527-1-2
Elongation at Yield 23 %23 %ISO 527-1-2
Flexural Strength 70.0 MPa10200 psiISO 178
Flexural Modulus 1.70 GPa247 ksiISO 178
Izod Impact, Notched (ISO) 33.0 kJ/m²15.7 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146/A
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 280 °C464 - 536 °FMolding
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 90.0 °C194 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL200 / 313108

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.