MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Llumar N1050 SR CDF (Neutral) Window Film
Categories: Polymer; Film

Material Notes: Neutral films reduce glare, provide moderate heat rejection, and are specified where a soft, neutral appearance is desired. These films are made with sputtered technology, creating a film that allows for very uniform visible light transmission. Neutral films are scratch-resistant and shield 99% of ultraviolet rays.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 50 %50 %
UV Transmittance 46 %46 %Solar
Reflection Coefficient, Visible (0-1) 0.110.11Visible Reflectance (interior)
 0.120.12Total Solar Reflectance
 0.140.14Visible Reflectance (exterior)
 
Descriptive Properties
% Glare Reduction44
% Summer Solar Heat Gain Reduction31
% Total Solar Energy Rejected41
% Ultraviolet Ray Protection (wavelengths 300-380nm)99
% Winter Heat Loss Reduction-3
Emissivity0.89
Light to solar gain (LSG)0.85
Shading coefficient0.68
Solar absorption42
Solar Heat Gain Coefficient0.59
U-value1.07Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5427 / 222621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.