MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® XE 4158 nat PA612  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are:
  • Very good hydrolysis resistance
  • Good heat stability
  • High UV- and weathering resistance
  • Super high cold impact strength
  • Good chemical resistance
  • Good surface finish
  • Good dimensional stability
  • Low density
Grilamid XE 4158 natural is suitable for the extrusion of profiles and tubes for applications in automotive and industrial markets. In addition it can be used for injection molding applications such as winter sport items for which high impact strength at low temperatures is required.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccISO 1183
Water Absorption 1.3 %ISO 62
Moisture Absorption 0.600 %ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65dry, 15s; ISO 868
 65conditioned, 15s; ISO 868
Tensile Strength, Yield 30.0 MPaconditioned; ISO 527-1/-2
 30.0 MPadry; ISO 527-1/-2
Elongation at Break >= 50 %conditioned; ISO 527-1/-2
 <= 50 %dry; ISO 527-1/-2
Elongation at Yield 13 %dry; ISO 527-1/-2
 18 %conditioned; ISO 527-1/-2
Tensile Modulus 750 MPaconditioned; ISO 527-1/-2
 1000 MPadry; ISO 527-1/-2
Charpy Impact Unnotched NBdry; ISO 179/1eU
 NBconditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
conditioned; ISO 179/1eU
Charpy Impact, Notched 85.0 kJ/m²dry; ISO 179/1eA
 85.0 kJ/m²conditioned; ISO 179/1eA
 40.0 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eA
 60.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmdry; IEC 60093
 1.00e+11 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 40.0 kV/mmdry; IEC 60243-1
 40.0 kV/mmconditioned; IEC 60243-1
Comparative Tracking Index 600 Vconditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 170 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 210 µm/m-°CISO 11359-1/-2
Melting Point 179 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 100 °Clong term; EMS
 150 °Cshort term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Cooling and climate control
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
 Other Extrusion
Product AttributesFlexible
 Hydrolysis resistant
 Improved alcohol resistance
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® Tieflex R463 NAT TL PA
Clariant Renol 612-01L Nylon 612, Lubricated
Evonik VESTAMID® D26 PA 612 Conditioned
EMS-Grivory Grilamid® XE 4208 black 9992 PA612-I
EMS-Grivory Grilamid® XE 4107 nat PA612-GF40

PGRH139 / 156848

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.