Sinpolene MBW0251 is a polyethylene-based pure white masterbatch designed specifically for use in tubular film blowing, blow molding and extrusion of polyolefins. With its high pigment loading, it offers high coloring value with excellent quality and performance. It is delivered as free flowing pellets for processing convenience. Characteristic: - Easy processing
- Good dispersion
- Good whiteness
Availability: Asia Pacific Filler/Reinforcement: Titanium Dioxide (Tio2), 25% Uses: Film; Sheet RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Blown Film; Sheet Extrusion; Blow Molding; Injection Molding Information provided by Teknor Apex |