Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C67600, H01 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/4 Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld; Fair Suitability – Gas Shielded Arc Welding; Poor Suitability – Capacity for Being Cold Worked

Typical Uses: Gate Valve Stems; Valve Balls; Welding Rod

Applicable Specifications: Brazing Filler Metal – AWS A5.8; Die Forging - Hot-Pressed ASTM B138/B138M; Forgings, Die (Hot Pressed) – ASTM B283/B283M, ASME SB283; Rod, Bar & Shapes – ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 83
@Thickness 25.4 mm
83
@Thickness 1.00 in
Tensile Strength 531 MPa77000 psi
Tensile Strength, Yield 310 MPa
@Thickness 25.4 mm
45000 psi
@Thickness 1.00 in
0.5% Ext
Elongation at Break >= 23 %
@Thickness 25.4 mm
>= 23 %
@Thickness 1.00 in
Tensile Modulus 103 GPa15000 ksi
Modulus of Rigidity 38.6 GPa5600 ksi
Poissons Ratio 0.340.34Calculated
Machinability 60 %60 %
Forgeability 80 %80 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000720 ohm-cm0.00000720 ohm-cm24% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.2 µm/m-°C
@Temperature 20.0 - 300 °C
11.8 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 8.79 W/m-K61.0 BTU-in/hr-ft²-°F
Melting Point 866 - 888 °C1590 - 1630 °F
Solidus 866 °C1590 °F
Liquidus 888 °C1630 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 57 - 60 %57 - 60 %
Iron, Fe 0.40 - 1.3 %0.40 - 1.3 %
Lead, Pb 0.50 - 1.0 %0.50 - 1.0 %
Manganese, Mn 0.050 - 0.50 %0.050 - 0.50 %
Tin, Sn 0.50 - 1.5 %0.50 - 1.5 %
Zinc, Zn 37 - 41.6 %37 - 41.6 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC67600x3 / 292346

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.