MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Tefzel® HT-2202 Fluoropolymer Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: DuPont™ Tefzel® HT-2202 fluoropolymer is a special-purpose resin available in 2.5-mm (0.1-in.) pellets. Tefzel® HT-2202 is a modified ETFE resin designed to promote adhesion between polyamide resins and ETFE resins.

Tefzel® HT-2202 and the other Tefzel® fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties.

Tefzel® HT-2202 is an easy-to-process adhesive material. Tefzel® HT-2202 is inert to most solvents and chemicals, hydrolytically stable, and weather resistant. Recommended upper service is 150°C (302°F); useful properties are retained at cryogenic ranges. The level and stability of dielectric properties are excellent. Mechanical properties include outstanding high-impact strength, cut-through, and abrasion resistance.

Applications

Tefzel® HT-2202 is ideal for many end products, including electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, multi-layer tubing, valves, containers, and fasteners; battery or instrument components that require chemical inertness; and mechanical parts.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Ethylene Tetrafluoroethylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Water Absorption 0.0070 %24 hours; ASTM D570
Melt Flow 7.0 g/10 minASTM D3159
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 35.0 MPaASTM D3159
Elongation at Break 250 %ASTM D3159
Flexural Modulus 1.0 GPaASTM D790
Izod Impact, Notched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 250 - 280 °CASTM D3159
Oxygen Index 30 - 32 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellent
Weather ResistanceExcellentYears unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Tefzel® HT-2190 Fluoropolymer Resin
Chemours Tefzel® HT-2183 Fluoropolymer Resin
Chemours Tefzel® HT-2127 Fluoropolymer Resin
Chemours Tefzel® HT-2170 Static Dissipating Semiconductive Resin
Chemours Tefzel® HT-2181 Fluoropolymer Resin

PDU929C / 33369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.