SUMILITERESIN®PR-311 is a powder novolac resin based on a phenolic novolac polymer. It is supplied in the form of powder for refractories, heat insulating material, or organic combination.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |