MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics GA-1050-OR3-LF PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Application: Lead free, 105° C PVC insulating compound designed for SJEOO applications. Complies with RoHS requirements.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 - 1.33 g/cc1.27 - 1.33 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 8678 - 86ASTM D2240
Tensile Strength 17.8 MPa2580 psiASTM D412
 15.66 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
2271 psi
@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
 15.66 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
2271 psi
@Treatment Temp. 140 °F,
Time 168 hour
Elongation at Break 280 %280 %ASTM D412
 291.2 %
@Treatment Temp. 136 °C,
Time 605000 sec
291.2 %
@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
 305.2 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
305.2 %
@Treatment Temp. 140 °F,
Time 168 hour
100% Modulus 9.65 MPa
@Strain 100 %
1400 psi
@Strain 100 %
ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmwet; ASTM D257
 5.00e+14 ohm-cm5.00e+14 ohm-cmdry; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -24.0 °C-11.2 °FASTM D746
Oxygen Index 27 %27 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aurora Plastics TufTech™ GA-1050 PVC Compound
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F
Arkema Lacovyl® PS 1050 PVC
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050

PSEPO023 / 140986

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.